The sophisticated combination

CREATION LS & LS PRESS –
Press, veneer and individualise with lithium disilicate!

Efficiency and natural aesthetics: Creation LS Press and Creation LS are a perfect ceramic symbiosis offering dental technicians reliability and stability but also brilliant colours and versatility on and with lithium disilicate, as standard is not enough for Creation!

Creation Willi Geller completes the product range with a new pressable and veneering ceramic allowing the dental technician outstanding aesthetics, whether used single or in combination. With the Creation LS Press blanks and the Creation LS veneering ceramic perfectly matched to the lithium disilicate frame highly aesthetic and stable all-ceramic restorations can be manufactured – efficiently pressed and then individually veneered resp. characterised with the proven CreaColor stains and modifiers.

Reliably combined for extended possibilities: the two system components Creation LS Press and Creation LS follow master ceramist Willi Geller’s “Simply Brilliant” philosophy proven for 30 years. They allow the dental technician manufacturing naturally beautiful anterior and posterior restorations with resp. on lithium disilicate assuring system safety.

SINGLE PRODUCTS
  • LS – BD-A
  • LS – D-A3
  • LS – E-58
  • LS – OD-32
  • LS Press – HT-3
  • LS Press – LT-A
  • LS Press – MO-2
  • LS Press – MT-B00
Sonia Cattazzo, Oral Design

CREATION LS –
the passion for the detail

Creation LS is a veneering ceramic especially developed for Creation LS Press.
It consists of an amorphous glass matrix replenished with feldspar. Thus Creation LS obtains a very natural light reflection combined with all advantages of the material technology for the veneering of lithium disilicate.
The colour assortment of Creation LS follows the proven colour coding concept of all veneering ceramics by Creation Willi Geller. Thus the Creation LS Press restorations can be veneered simply and efficiently according to the usual layering concept. 

CREATION LS PRESS –
for good reason!

Creation LS press blanks are produced in a special technical process in which lithium disilicate crystals are embedded in a glass matrix. The special characteristic is the homogenous distribution and the high filling level of microcrystalline lithium disilicate. The results are outstanding material properties and natural aesthetics of the restorations.

THE BRILLIANCE OF THE CREATION LS:

  • Comprehensive colour assortment for individual veneering and characterisation
  • Layer build-up according to the tried-and-tested colour coding concept of Creation
  • Natural colour brilliance and light effects due to feldspar content
  • Homogeneous crystal structure and outstanding surface density

THE BRILLIANCE OF CREATION LS PRESS:

  • High strength due to homogeneous crystalline structure: > 500 MPa
  • Minimal invasive preparation: 0.3 mm veneer, 0.8 mm anterior
  • Creative freedom of manufacturing: full veneers, partial veneers
  • The appropriate blank for every indication

Firing chart

The above firing parameters are guide values which must always be adapted to the furnace being used and the situation of the furnace. Getting the right firing result is what matters.

Press programmes

Color chart

 

 

Colour chart

CREATION LS

Vita® is a registered trade mark of VITA Zahnfabrik H. Rauter GmbH & Co. KG, Bad Säckingen, Germany.

 

 

Materials which are not related to the Vita®shade guide:

 

CREATION LS PRESS

Vita® is a registered trade mark of VITA Zahnfabrik H. Rauter GmbH & Co. KG, Bad Säckingen, Germany.

 

 

Materials which are not related to the Vita®shade guide:

Creation LS Press blank MO (Medium Opacity)
Well suitable for covering discoloured dies and titanium abutments as well as fully veneered restorations due to the good light reflection and brightness.

Creation LS Press blank LT (Low Translucency)
Can be used for the cut-back as well as for partially veneered crowns with subsequent veneering with Creation LS, but also shows good opacity for fully veneered restorations with minimal layer thicknesses.

Creation LS Press blank MT (Medium Translucency)
Ideal for fully anatomical restorations with individual shade adjustment in the staining technique (Make up Neo) but also for the cut-back technique or fully veneered restorations – with subsequent individualisation with Creation LS.

Creation LS Press blank HT (High Translucency)
To create small and minimal invasive restorations where mainly the natural enamel is replaced, e.g. inlays, onlays and veneers. The shade individualisation is carried out in the staining technique (Make up Neo).

Physical properties

The stated technical and physical values relate to samples prepared in-house and the measuring instruments located in-house.

Processing techniques

 

 

Preparation guidelines Creation LS Press

  • The preparations should have no angles or sharp edges
  • The ideal preparation form is a chamfer or step preparation with a rounded shoulder
  • The substance removal of the tooth should not fall below the dimensions of the restoration's minimum wall thickness
  • The preparation margins must not be in contact with theantagonist
  • The preparation corresponds to a reduced shape
  • The preparation should have a retentive shape as well as a preparation angle of 6 to 10 °
  • Ensure a sufficient preparation height

Tangential preparations, thin outlet preparations or deep chamferpreparations with undercuts are not suitable.

  • Reducing the anatomical shape in the occlusal area by 1.0 mm
  • No preparation of undercut areas
  • The preparation angle of the cavity wall towards the tooth axis should form an angle of 6 °
  • All internal edges and angles should be rounded
  • Do not prepare feather edges
  • There must be a preparation depth of at least 1.0 mm and an isthmus width in the area of the fissures of at least 1.0 mm
  • No preparation of undercut areas
  • The preparation angle of the cavity wall towards the tooth axis should form an angle of 6 °
  • Do not prepare a tooth with feather edges
  • All internal edges and angles should be rounded
  • Reducing the labial area by at least 0.3 mm and the cutting edge by at least 0.4 mm
  • The reduction of the substance should be in the enamel area
  • Do not prepare a tooth with feather edges
  • The incisal edge should be reduced by about 1.5 mm
  • The reduction in the body (vestibular, interdental, palatal) should be 1.2 mm
  • The width of the shoulder/chamfering should be at least 1.0 mm
  • Reducing the anatomical shape in the occlusal area by 1.5 mm
  • Reducing the crown in the circular area by at least 1.0 mm
  • The cusps and edges must be rounded

Downloads

All kits at a glance
  • LS Kit
    Basic and effect porcelains with the tooth shades BD-A, BD-B, BD-B0, A1, A2, A3, A3.5, B1, B2, B3, C2, D2
  • LS Press Starter Kit
    Introduction Kit
  • LS Press Introduction Kit A1, A2
    The easy introduction of the system
  • LS Press Introduction Kit A3
    The easy introduction of the system